Specifications
Normal temperature Frequency Tolerance:
±10ppm
Frequency Stability:
±30ppm
Operating Temperature:
-40℃~+85℃
Load Capacitance:
9pF
Frequency:
40MHz
Mfr. Part #:
7U40000E09UCG
Package:
SMD3225-4P
Key Attributes
Model Number: 7U40000E09UCG
Product Description

Product Overview

The 7U Series Quartz Crystal Unit is a seam-sealed ceramic surface mount package designed for reliable frequency control. It offers a compact 3.2*2.5mm footprint, making it suitable for various electronic applications requiring precise timing.

Product Attributes

  • Brand: SJK ()
  • Origin: Shenzhen, China
  • Certifications: RoHS, REACH, HF
  • Package Type: 3.2*2.5mm Surface Mount, Ceramic, Seam Sealed
  • Minimum Packaging: 3000pcs/real
  • Moisture Sensitivity Level: Level 1

Technical Specifications

ParameterSpecification
Output Frequency40.000000MHz
ModeAT/Fundamental Frequency
Frequency Tolerance (@25C)10 ppm max
Load Capacitance (CL)9.0 PF
Frequency Stability Over Operating Temperature10ppm max / -20 C to +70 C
30ppm max/ -40 C to +85 C
Operating Temperature Range-40 C to +85 C
Storage Temperature Range-40 C to +125 C
Shunt Capacitance (C0)3.0 PF Max
Driver Level (Typical)10W
Equivalent Series Resistance (ESR)40 Max
Aging @25C (1st year Max)3ppm/year
Testing ConditionsAmbient temperature: 255
Relative humidity: 40%~70%
Measure equipment: S&A250B or equivalent

Reliability Test Specification

No.Test ItemTest ConditionStandard Requirement
1DropFree fall from 55cm height onto a wooden board, 3 timesFrequency change within 5ppm, resistance change within 15% before and after test
2VibrationFrequency: 10~55Hz, Amplitude: 1.5mm, Time: 2 hours per direction (X, Y, Z)Frequency change within 5ppm, resistance change within 15% before and after test
3Thermal Shock25 cycles of high and low temperature in a test chamber. Low temp: -403 for 30 min, High temp: 852 for 30 min. Transition time: 3 minutes.Frequency change within 5ppm, resistance change within 15% before and after test
4HermeticityHelium pressure: 50.5Kg/cm, Helium pressurization time: 120 minutesLeak rate: 110-9Pa.m3/s
5Resistance to Soldering HeatWave crest temperature: 260C10C, Time: 155 secondsFrequency change within 5ppm, resistance change within 15% before and after test
6Solderability TestTemperature: 260C10C, Immersion time: 31 secondsSoldered area coverage of pins 90%
7High Temperature & HumidityTemperature: 60C2C, Humidity: 90%~95%, Duration: 240 hours1. Frequency change within 5ppm, resistance change within 15% before and after test.
2. Product surface should not be rusted.
8High Temperature TestTemperature: 85C2C, Duration: 240 hoursFrequency change within 5ppm, resistance change within 15% before and after test
9Low Temperature TestTemperature: -40C2C, Duration: 240 hoursFrequency change within 5ppm, resistance change within 15% before and after test
10Life TestVoltage: 5V, Temperature: 25, Duration: 1000 hoursFrequency change within 5ppm, resistance change within 15% before and after test

2207271530_SJK-7U40000E09UCG_C524769.pdf

Request A Quote

Please Use Our Online Inquiry Contact Form Below If You Have Any Questions, Our Team Will Get Back To You As Soon As Possible

You Can Upload Up To 5 Files And Each File Sized 10M Max