Specifications
Voltage Rating:
10V
Capacitance:
10nF
Temperature Coefficient:
X7R
Tolerance:
±10%
Mfr. Part #:
GRM033R71A103KA01D
Package:
0201
Key Attributes
Model Number:
GRM033R71A103KA01D
Product Description
Product Overview
Chip Multilayer Ceramic Capacitors for General Electronic Equipment. This product specification applies to general-purpose chip multilayer ceramic capacitors.
Product Attributes
- Brand: MURATA
Technical Specifications
| Part Number | Size Code | Temperature Characteristics | Rated Voltage | Nominal Capacitance | Capacitance Tolerance | Packaging | Packaging Code |
| GRM033R71A103KA01 | 0201 | X7R (EIA) | DC 10 V | 10000pF | +/-10% | 15000 pcs./Reel (180mm Reel PAPER Tape) | D |
| GRM033R71A103KA01 | 0201 | X7R (EIA) | DC 10 V | 10000pF | +/-10% | 30000 pcs./Reel (180mm Reel PAPER Tape) | W |
| GRM033R71A103KA01 | 0201 | X7R (EIA) | DC 10 V | 10000pF | +/-10% | 50000 pcs./Reel (330mm Reel PAPER Tape) | J |
| Item | Specification | Test Method (Ref. Standard:JIS C 5101, IEC60384) |
| Rated Voltage | Defined as the maximum voltage which may be applied continuously to the capacitor. | Shown in Rated value. |
| Appearance | No defects or abnormalities. | Visual inspection. |
| Dimension | Refer to Rated value. | Using Measuring instrument of dimension. |
| Voltage Proof | No defects or abnormalities. | Test Voltage : 250% of the rated voltage, Applied Time : 1s to 5s, Charge/Discharge Current : 50mA max. |
| Insulation Resistance(I.R.) | More than 10000M | Measurement Temperature:Room Temperature, Measurement Point : Between the terminations, Measurement Voltage : Rated Voltage, Charging Time : 2min, Charge/Discharge Current : 50mA max. |
| Capacitance | Shown in Rated value. | Measurement Temperature:Room Temperature, Measurement Frequency : 1.0+/-0.1kHz, Measurement Voltage : 1.0+/-0.2Vrms |
| Q or Dissipation Factor (D.F.) | DF:0.035 max. | Measurement Temperature : Room Temperature, Measurement Frequency : 1.0+/-0.1kHz, Measurement Voltage : 1.0+/-0.2Vrms |
| Capacitance Change (Temperature Characteristics) | Within +/-15% (at -55 to +125) | Measurement Voltage : Less than 1.0Vrms, Pre-treatment : Heat treatment at 150+0/-10C for 1hour and then sit for 24+/-2hours at room temperature. |
| Adhesive Strength of Termination | No removal of the terminations or other defect should occur. | Solder the capacitor on the test substrate. Applied Force : 2N, Holding Time : 10+/-1s, Applied Direction : In parallel with the test substrate and vertical with the capacitor side. |
| Vibration | Appearance: No defects or abnormalities. Capacitance: Within the specified initial value. Q or D.F.: Within the specified initial value. | Solder the capacitor on the test substrate. Kind of Vibration : Simple harmonic motion 10Hz to 55Hz to 10Hz, Vibration Time : 1min, Total Amplitude : 1.5mm. Applied for 2 hours in each of 3 mutually perpendicular directions (total of 6 hours). |
| Substrate Bending Test | Appearance: No defects or abnormalities. Capacitance: Within +/-10% | Solder the capacitor on the test substrate. Flexure : 1mm, Holding Time : 5+/-1s. |
| Solderability | 95% of the terminations is to be soldered evenly and continuously. | Solder bath method, Flux : Solution of rosin ethanol 25(mass)%, Preheat : 80 to 12010s to 30s, Solder : Sn-3.0Ag-0.5Cu(Lead Free Solder), Test Temp. : 245+/-5, Test Time : 2+/-0.5s. |
| Resistance to Soldering Heat | Appearance: No defects or abnormalities. Capacitance Change: Within +/-7.5%. Q or D.F.: Within the specified initial value. I.R.: Within the specified initial value. Voltage Proof: No defects. | Solder bath method, Solder : Sn-3.0Ag-0.5Cu(Lead Free Solder), Solder Temp. : 270+/-5, Test Time : 10+/-0.5s, Preheat Temp. : 120 to 150, Preheat Time : 1min. Post-treatment : Let sit for 24+/-2hours at room temperature. |
| Temperature Sudden Change | Appearance: No defects or abnormalities. Capacitance: Within +/-7.5%. Q or D.F.: Within the specified initial value. I.R.: Within the specified initial value. Voltage Proof: No defects. | Solder the capacitor on the test substrate. Cycles : 5 cycles. Pre-treatment : Heat treatment at 150+0/-10C for 1hour and then sit for 24+/-2hours at room temperature. Post-treatment : Let sit for 24+/-2hours at room temperature. |
| High Temperature High Humidity (Steady) | Appearance: No defects or abnormalities. Capacitance: Within +/-12.5%. Q or D.F.: DF:0.05 max. I.R.: More than 500M or 25F (Whichever is smaller). | Solder the capacitor on the test substrate. Test Temperature : 40+/-2, Test Humidity : 90%RH to 95%RH (Steady), Test Time : 500+/-12h, Test Voltage : Rated Voltage. Post-treatment : Let sit for 24+/-2hours at room temperature. |
| Durability | Appearance: No defects or abnormalities. Capacitance: Within +/-12.5%. Q or D.F.: DF:0.05 max. I.R.: More than 1000M or 50F (Whichever is smaller). | Solder the capacitor on the test substrate. Test Temperature : Maximum Operating Temperature+/-3, Test Time : 1000+/-12h, Test Voltage : 200% of the rated voltage. Pre-treatment : Apply test voltage at test temperature for 1hour and then sit for 24+/-2hours at room temperature. Post-treatment : Let sit for 24+/-2hours at room temperature. |
2410121857_muRata-GRM033R71A103KA01D_C76941.pdf