Online Service

Online Service

Contact Person
+86 136 6733 2386
quality multilayer ceramic capacitor HRE CGA0402X5R475M250GT rated at 25 volts with X5R dielectric material factory
<
quality multilayer ceramic capacitor HRE CGA0402X5R475M250GT rated at 25 volts with X5R dielectric material factory
>
Specifications
Voltage Rating:
25V
Capacitance:
4.7uF
Temperature Coefficient:
X5R
Tolerance:
±20%
Mfr. Part #:
CGA0402X5R475M250GT
Package:
0402
Key Attributes
Model Number: CGA0402X5R475M250GT
Product Description

Product Overview

This product specification applies to multilayer ceramic capacitors. These capacitors are designed for various electronic applications requiring stable capacitance and reliable performance.

Product Attributes

  • Brand: Not specified
  • Origin: Not specified
  • Material: Dielectric ceramic, Nickel inner electrode, Copper outer electrode, Tin plating
  • Color: Not specified
  • Certifications: Not specified

Technical Specifications

ItemSpecificationTest Method
Capacitance15% (X5R)JIS C 5101, IEC60384
Capacitance Tolerance15% (X5R)JIS C 5101, IEC60384
Rated Voltage25VdcJIS C 5101, IEC60384
Temperature CharacteristicX5R: -55 to +85, 15% capacitance changeJIS C 5101, IEC60384
Dimensions (mm)Length: 1.00+0.20/-0.05, Width: 0.50+0.20/-0.05, Thickness: 0.15-0.35JIS C 5101, IEC60384
Insulation Resistance (I.R.) 10 G or RC 500F (whichever is smaller)JIS C 5101, IEC60384
Voltage ProofWithstand test voltage without defects or abnormalities.JIS C 5101, IEC60384
AppearanceNo defects or abnormalities. Visual (microscope) inspection.JIS C 5101, IEC60384
DimensionsConform to specifications. Micrometer inspection of physical dimensions.JIS C 5101, IEC60384
Substrate Bending TestNo terminal peeling, ceramic breakage, etc. Force: 2.5N (for 0402 size). Bend 1mm after reflow soldering.JIS C 5101, IEC60384
Adhesive Strength of TerminationNo terminal peeling, ceramic breakage, etc.JIS C 5101, IEC60384
Solderability95% of terminals should be uniformly and continuously soldered.JIS C 5101, IEC60384
Resistance to Soldering HeatNo cracks in appearance.JIS C 5101, IEC60384
Temperature Cycle5 cycles. No defects or abnormalities. Capacitance change: X7R/X5R: 15%JIS C 5101, IEC60384
Durability Test100012 hours at rated voltage. Capacitance change: X7R/X5R: 12.5%. Insulation Resistance: 1G or R.C 50s (for X5R).JIS C 5101, IEC60384
High Temperature High Humidity Test50024 hours at 402, 90%-95%RH. Capacitance change: X7R/X5R: 12.5%. Insulation Resistance: 1G or R.C 50s (for X5R).JIS C 5101, IEC60384
Packaging180mm reel, paper tape. 10,000 pcs/reel.N/A

2410080906_HRE-CGA0402X5R475M250GT_C6119795.pdf

Request A Quote

Please Use Our Online Inquiry Contact Form Below If You Have Any Questions, Our Team Will Get Back To You As Soon As Possible

You Can Upload Up To 5 Files And Each File Sized 10M Max