Product Overview
The CBB21/MPP series metallized polypropylene film capacitors are designed for electronic equipment with epoxy encapsulation. These capacitors feature a non-inductive winding structure with metallized polypropylene film and tin-plated copper wire leads. They are suitable for DC blocking, coupling, decoupling, filtering, bypassing, and other high-frequency, DC, AC, and pulse circuits. Key advantages include excellent self-healing properties, low loss, and low internal temperature rise, all encapsulated in flame-retardant epoxy resin powder coating.
Product Attributes
- Product Type: Metallized Polypropylene Film Capacitor (Impregnated Type)
- Series: CBB21/MPP
- Encapsulation: Epoxy resin powder coating (Flame-retardant UL94V-0)
- Origin: Dongguan City Chengxi Electronics Co., Ltd.
- Certifications: RoHS, REACH, Halogen-free (if required)
Technical Specifications
| Product Code | Capacitance | Tolerance | Rated Voltage (V.dc) | Pitch (mm) | Dimensions (mm) (W x H x T) | Lead Diameter (d) |
|---|---|---|---|---|---|---|
| MPP204J2JD070C3F0ZR | 0.01F | 5% | 630V | 15.0 | 16.7 x 12.0 x 6.8 | 0.6 |
General Electrical Characteristics
| Parameter | Specification | Test Conditions |
|---|---|---|
| Climate Category | 40/105/21 | |
| Operating Temperature Range | -40 to +105 | (Voltage derating of 1.25% / for +85 to +105) |
| Rated Temperature | 85 | |
| Capacitance Range | 0.001F to 6.8F | |
| Capacitance Tolerance | 5% (J), 10% (K) | |
| Rated Voltage (Vdc) | 100, 160, 250, 400, 630, 1000, 1250, 1600, 2000 | |
| Dissipation Factor (DF) | 0.0010 | (1kHz, 20) |
| Insulation Resistance | 30,000M (for C0.33uF) | (100VDC, 60 seconds) |
| Insulation Resistance | 10000M*uF (for C>0.33uF) | (100VDC, 60 seconds) |
| Withstand Voltage | 1.6 UR(VDC) | 5 seconds |
Maximum Pulse Rise Rate (dV/dt)
| dV/dt (V/s) | UR (VDC) | Pitch 7.5mm | Pitch 10.0mm | Pitch 15.0mm | Pitch 22.5mm | Pitch 27.5mm |
|---|---|---|---|---|---|---|
| 100/160 | 130 | 110 | 100 | 70 | 50 | |
| 250 | 240 | 220 | 200 | 120 | 100 | |
| 400 | 450 | 350 | 300 | 180 | 150 | |
| 630 | 550 | 420 | 400 | 250 | 180 | |
| 1000/1250 | 2300 | 1950 | 975 | 600 | 300 | |
| 1600 | / | 6000 | 4500 | 2400 | / | |
| 2000 | / | / | 8000 | 4500 | / |
Note: If the actual working voltage (U) is lower than the rated voltage (UR), the capacitor can operate at a higher dV/dt. The allowable dV/dt value should be multiplied by UR/U.
Product Structure and Main Materials
| No. | Main Material | Description | Remarks |
|---|---|---|---|
| 1 | Metallized Polypropylene Film | MPPZAH | -/- |
| 2 | Spray Plating Layer | Zinc-tin alloy wire | -/- |
| 3 | Leads | Tin-plated copper-clad steel wire | -/- |
| 4 | Outer Encapsulation Material | Epoxy resin powder | Flame-retardant UL94-0 |
| 5 | Inner Protective Material | Epoxy resin |
Note: All raw materials and finished products comply with RoHS environmental requirements.
Packaging Information
| Item | Details |
|---|---|
| Inner Box Dimensions (L*W*H) | 34.5*23.5*24.5 cm |
| Outer Box Dimensions (L*W*H) | 49*36*27 cm |
| Box Content Details | Manufacturer part number, number of packages and quantity per package, Lot No. |
| Packaging Material | Transparent PVC bag for moisture and dust protection |
| Labeling | Manufacturer logo (DGCX), Product model or code (MPP), Rated capacitance and tolerance (e.g., 224J), Rated voltage (e.g., 400V), RoHS environmental mark, Other customer specified requirements. |
Storage Conditions
| Parameter | Specification |
|---|---|
| Temperature | Max 35 |
| Relative Humidity | Max 80% |
| Storage Duration | Maximum 12 months (from production date marked on the packaging bag) |
Note: Prolonged exposure to air may degrade lead solderability. Avoid high temperature and high humidity environments.
Soldering Rules
| Soldering Method | Temperature/Time Specifications |
|---|---|
| Wave Soldering (MPP Polypropylene Film Capacitors) | Preheating section (Ts): Max 120, 45 seconds Peak temperature (Tp): Max 110, 120 seconds For P7.5mm, T4mm: Soldering time < 4 seconds |
| Soldering Iron | Tip temperature: Max 350, Time: Max 3 seconds |
Note: Lead-type film capacitors are not suitable for reflow soldering.
2512091725_DGCX-MPP204J2JD070C3F0ZR_C53133390.pdf
Please Use Our Online Inquiry Contact Form Below If You Have Any Questions, Our Team Will Get Back To You As Soon As Possible